Ferro Frit 4124

Hard calcium borate frit

Alternate Names: Frit DA4124

OxideAnalysisFormula
CaO14.15%0.677
K2O1.26%0.036
Na2O6.63%0.287
Al2O35.96%0.157
B2O314.42%0.556
SiO257.56%2.570
Oxide Weight268.34
Formula Weight268.34
This is the chemistry of the material (the formula compares numbers of molecules, the analysis compares them by weight). In glazes, the composite chemistry of the mix is the main factor shaping fired properties (e.g. color, melting temperature, surface). In bodies we are interested in their physical properties (e.g. shrinkage, porosity, strength), these are a product of the mineralogy of the materials.
GSPT - Softening Point 577C
MLRG - Melting Range (C) 1040-1100C
GTTM - Glass Transition Temperature 622C

Suitable for glazes used over underglaze colors.
This is similar to Ferro Frit 3124 but has less Al2O3.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4124" descrip="Hard calcium borate frit" searchkey="Frit DA4124" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="14.153" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="U" percent="1.263" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="6.631" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.967" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.421" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.561" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 https://digitalfire.com, All Rights Reserved