Ferro Frit 3481

Medium lead calcium cone 06-02 frit for chrome tin colors

Alternate Names: F3481

OxideAnalysisFormula
CaO9.90%0.52
K2O1.19%0.037
Na2O3.09%0.15
PbO22.77%0.30
Al2O37.00%0.20
B2O36.20%0.26
SiO249.86%2.43
Enter the formula and formula weight directly into the Insight MDT dialog (since it records materials as formulas).
Enter the analysis into an Insight recipe and enter the LOI using Override Calculated LOI (in the Calc menu). It will calculate the formula.
COLE - Co-efficient of Linear Expansion 7.5
MLRG - Melting Range (C) 1600F

Made from flint, borax, calcium, clay and lead.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3481" descrip="Medium lead calcium cone 06-02 frit for chrome tin colors" searchkey="F3481" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="9.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="U" percent="1.190" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="3.090" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="U" percent="22.770" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.860" tolerance=""/> </oxides> </material>
The future of ceramic recipe, material and physical testing record keeping is here. Just pennies a day.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipes and materials on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Import existing material, recipe data.
  • As many side-by-side recipes and/or materials as you want (chemistry is shown for all).
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, pictures with individual titles and descriptions, material links.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to materials, typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to recipe imports (later search by batch).
  • Assign multiple typecodes to imported glaze and body batches (to classify) (search on these later).
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding recipe records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.
  • Import materials data in various formats or just use the thousands of built-in reference materials.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()

0