Ferro Frit 3289

High barium leadless frit for bright colors, satin finishes

Alternate Names: F3289

OxideAnalysisFormula
BaO27.40%0.668
Na2O5.50%0.332
Al2O35.40%0.198
B2O312.40%0.666
SiO249.30%3.067
Oxide Weight373.91
Formula Weight373.91
This is the chemistry of the material (the formula compares numbers of molecules, the analysis compares them by weight). In glazes, the composite chemistry of the mix is the main factor shaping fired properties (e.g. color, melting temperature, surface). In bodies we are interested in their physical properties (e.g. shrinkage, porosity, strength), these are a product of the mineralogy of the materials.
COLE - Co-efficient of Linear Expansion 8.20
MLRG - Melting Range (C) 1500F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3289" descrip="High barium leadless frit for bright colors, satin finishes" searchkey="F3289" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="27.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.300" tolerance=""/> </oxides> </material>