Barium Carbonate


Barium carbonate powder is well known as a poisonous substance whereas barium sulfate is insoluble and non-toxic. Barium carbonate performs certain physical and oxide sourcing functions in ceramic glazes and bodies for which substitutes can be either very difficult or expensive to implement. Determining the threat of barium is not as simple as simply saying "all uses of barium are dangerous". Barium carbonate supplies BaO to glazes which may or may not be soluble in acids that come into contact with the glaze surface. This solubility depends on the chemical balance of the glaze, that is, the degree to which it locks the BaO molecules into the glass structure. In bodies, minute percentages of barium carbonate precipitate soluble salts that cause surface scumming in fired ware and no other material is known to effectively perform this function. Thus discussions of barium toxicity relate to the actual use of the powder in the studio or plant and the degree of solubility of ware made using barium compounds.

Where barium carbonate is employed for chemistry reasons, hazards related to its raw form can be minimized by using a frit that sources barium oxide. This involves doing chemistry calculations to introduce the frit without changing the overall chemistry of the glaze.

Harzards related to the quality of ware produced are not connected to the material sourcing the BaO, but to the availability of BaO ions to solubility. This can be a complex issue and tradeoffs must be considered. Where small percentages are involved, the likelihood of danger is also small if the glaze is balanced (e.g. well melted and having adequate silica and alumina). But at the same time small amounts are likely candidates for substitution with other fluxing oxides without significant effects on physical properties or appearance of the glaze. Where larger amounts are involved successful substitution is much less likely. Crystalline matte surfaces done with barium, for example, often have a character that is difficult to duplicate with other oxides. For example, there are many frits intended for the production of matte glazes that employ BaO as the mechanism. One alternative is to develop a base matte glaze using another mechanism (i.e. high CaO, SrO) and substitute the colorants, opacifiers and variegators into it. The presence of barium is key to the development of certain colors (e.g. barium blue) and substitution of other oxides often will not work.

It is possible to achieve barium-unique effects and still have a glaze that has low solubility. However most would agree to the ethical position that such glazes should not be used on food surfaces without additional leach testing on over and underfired ware. Even then the possibility that a glaze has a fragile chemical balance that protects leachability presents the possibility that small variations in materials could disproportionately increase solubility at times.

For more information, check the article links for the barium carbonate at www.ceramicmaterials.info. These provide detailed toxicity data and information about the use of barium to precipitate soluble salts in clay bodies.

One final note: Barium is considered dangerous when swallowed, however it is much less toxic as dust or in skin contact. The author has worked in a local ceramic industry that has routinely used barium carbonate in tile, brick and pottery bodies for 90 years and the silicosis threat from quartz in the clay has always completely overshadowed toxicity ingestion or inhalation issues surrounding barium.

Out Bound Links

In Bound Links




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()