GC106 Base Fara Shimbo Crystalline Glaze

Start temperature assumed: 25°C
Step Rate to Temp °C Rate
°F/hr
To °F Hold Accum
Time
1 100°C/hr to 200 180 392 0 2:02  
2 250°C/hr to 500 450 932 0 3:14  
3 500°C/hr to 1275 900 2327 0 4:47  
4 9999°C/hr to 1130 17998 2066 15min 5:03  
5 30°C/hr to 1075 54 1967 0 6:53  
*Rates are expressed as "Celcius/Fahrenheit degrees", temperatures as "Degrees celcius/fahrenheit"

Out Bound Links

In Bound Links


By Tony Hansen

You should always be testing. But it is wasted without an audit trail. Document your lifetime of recipes, firing schedules, test results, pictures and much more in a private account at insight-live.com. It is the future, the next step after desktop Digitalfire Insight.

Watch videos, learn more, sign-up at http://insight-live.com.



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()

0